基于机器学习的生物可降解锌合金力学性能预测 |
| 郭传平, 石尘尘, 刘鹏, 高冬芳, 赵洋洋, 乔阳 |
|
Prediction of Mechanical Properties of Biodegradable Zinc Alloys Based on Machine Learning |
| GUO Chuanping, SHI Chenchen, LIU Peng, GAO Dongfang, ZHAO Yangyang, QIAO Yang |
| 图2 使用平均值和标准差扩展数据流程图 |
| Fig.2 Flowcharts for data extension using mean and standard deviation methods (IP and OP are matrices of input and output variables, respectively; i, j, and k are the number of data points, input variables, and output variables, respectively; SD is standard deviation) |
|