基于机器学习的生物可降解锌合金力学性能预测 |
| 郭传平, 石尘尘, 刘鹏, 高冬芳, 赵洋洋, 乔阳 |
|
Prediction of Mechanical Properties of Biodegradable Zinc Alloys Based on Machine Learning |
| GUO Chuanping, SHI Chenchen, LIU Peng, GAO Dongfang, ZHAO Yangyang, QIAO Yang |
| 图1 Zn、Mg和Mn混合粉末的DSC曲线及烧结工艺曲线 |
| Fig.1 DSC curves (a, b) and sintering process curve (c) of mixed powders (a) Zn-Mg hybrid powder (b, c) Zn-Mg-Mn hybrid powder |
|