基于随机森林算法与数据增强策略双驱动的多尺度疲劳裂纹扩展预测
刁圣轩, 肖金雍, 陈永保, 单康中, 杨杰

Multi-Scale Fatigue Crack Propagation Prediction Based on the Dual Drive of Random Forest Algorithm and Data Augmentation Strategy
DIAO Shengxuan, XIAO Jinyong, CHEN Yongbao, SHAN Kangzhong, YANG Jie
图8 350 MPa下基于双驱动模型和随机森林(RF)算法模型的多尺度疲劳裂纹扩展预测结果
Fig.8 Prediction results of multi-scale fatigue crack propagation at 350 MPa based on dual-drive model and RF model
(a) training results of training sets (b) prediction results of testing sets