螺旋桨铜合金的微观结构定量解析及深海压力下的失效动力学机制 |
| 杨慧敏, 李瑞雪, 周晨曦, 马宇轩, 赵旭辉, 雍兴跃, 刘景军 |
|
Effect of Seawater Pressures on Microstructure Quantitative Analysis and Failure Dynamics Mechanism of Copper Alloys for Ship Propellers |
| YANG Huimin, LI Ruixue, ZHOU Chenxi, MA Yuxuan, ZHAO Xuhui, YONG Xingyue, LIU Jingjun |
| 图7 基于不同海水压力下H2O分子与合金表面距离变化建立的Cl-吸附的MAB-Alseg合金模型及溶解过程腐蚀动力学参数分析 |
| Fig.7 Schematic of MAB-Alseg alloy model with by Cl- adsorption (a), adsorption energy at stable adsorption site (top of Al atom) on the surface of MAB-Alseg alloy (b), binding energy (Eb) between Cl- adsorption layer and matrix (c), work function of MAB-Alseg alloy after Cl- adsorption (d), energy diagram of Cu atom migration-dissolution processes of MAB-Alseg alloy after Cl- adsorption (e), and k of Cu atoms (f) at different seawater pressures |
|