螺旋桨铜合金的微观结构定量解析及深海压力下的失效动力学机制 |
| 杨慧敏, 李瑞雪, 周晨曦, 马宇轩, 赵旭辉, 雍兴跃, 刘景军 |
|
Effect of Seawater Pressures on Microstructure Quantitative Analysis and Failure Dynamics Mechanism of Copper Alloys for Ship Propellers |
| YANG Huimin, LI Ruixue, ZHOU Chenxi, MA Yuxuan, ZHAO Xuhui, YONG Xingyue, LIU Jingjun |
| 图4 不同海水压力下MAB合金腐蚀10 h前后的宏观形貌及SEM像 |
| Fig.4 Macroscopic corrosion morphologies of MAB alloy before and after corrosion for 10 h under different seawater pressures (a); SEM images of MAB alloys before corrosion (b) and after corrosion for 10 h under 0.1 MPa (c), 4.0 MPa (d), 6.0 MPa (e), 8.0 MPa (f), and 10.0 MPa (g) seawater pressures |
|