螺旋桨铜合金的微观结构定量解析及深海压力下的失效动力学机制
杨慧敏, 李瑞雪, 周晨曦, 马宇轩, 赵旭辉, 雍兴跃, 刘景军

Effect of Seawater Pressures on Microstructure Quantitative Analysis and Failure Dynamics Mechanism of Copper Alloys for Ship Propellers
YANG Huimin, LI Ruixue, ZHOU Chenxi, MA Yuxuan, ZHAO Xuhui, YONG Xingyue, LIU Jingjun
图3 MAB-Alseg合金表层Cu原子迁移-溶解的动力学过程示意图及各阶段Cu原子溶解的能量图
Fig.3 Processes of surface Cu atom migration-dissolution of MAB-Alseg alloy (Black dotted circles represent Cu atomic vacancies. IS—initial state, VAC1—surface vacancy, TS—transition state, VAC2—subsurface vacancy, FS—final state (two-vacancy structure)) (a) and energy diagram of each step in the dynamic process of Cu atom migration-dissolution (b) in the MAB-Alseg alloy (RDS—rate determining step, ΔEvac1—vacancy formation energy of the surface Cu atom, ΔEvac2—vacancy formation energy of the subsurface Cu atom)