螺旋桨铜合金的微观结构定量解析及深海压力下的失效动力学机制
杨慧敏, 李瑞雪, 周晨曦, 马宇轩, 赵旭辉, 雍兴跃, 刘景军

Effect of Seawater Pressures on Microstructure Quantitative Analysis and Failure Dynamics Mechanism of Copper Alloys for Ship Propellers
YANG Huimin, LI Ruixue, ZHOU Chenxi, MA Yuxuan, ZHAO Xuhui, YONG Xingyue, LIU Jingjun
图2 MAB合金和MAB-Alseg合金的晶格结构和内应力分析
Fig.2 Analyses of lattice structures and internal stresses of MAB (a-i) and MAB-Alseg (j-l) alloys
(a) refined XRD pattern (Rp—profile R-factor, Rwp—weighted profile R-factor, X2—Chi-squared)
(b, c) microstrains (b) and dislocation densities (c) of different crystal planes
(d, e) HRTEM image (d) and the corresponding inverse fast Fouries transform (IFFT) image (e) (Inset in Fig.2e is corresponding fast Fouries transform (FFT) patterns, red circle repre-sents [111] crystal orientation)
(f) statistical diagram of (111) lattice space (d)
(g-i) strain/stress field maps in the x direction (g), y direction (h), and xy direction (i) (Rectangle areas refer to dipoles)
(j-l) radial distribution functions of surface (j), subsurface (k), and matrix (l) regions (g(r) is the relative density of atoms or molecules)