类竹纤维结构TiB/Ti复合材料设计、制备与强韧化机制 |
||||||||||||||||||
| 魏子超, 吴华舵, 黄光法, 乐建温, 吕维洁, 韩远飞 | ||||||||||||||||||
|
Design and Fabrication of Bamboo-Fiber-Like TiB/Ti Composites with Strengthening and Toughening Mechanisms |
||||||||||||||||||
| WEI Zichao, WU Huaduo, HUANG Guangfa, LE Jianwen, LV Weijie, HAN Yuanfei | ||||||||||||||||||
| 表1 HS-4%、FLSCR-10%复合材料的理论强化效果 |
||||||||||||||||||
| Table 1 Theoretical strengthening effects of HS-4% and FLSCR-10% composites |
||||||||||||||||||
|
||||||||||||||||||