纳米晶304不锈钢板材的微观组织、显微硬度与耐腐蚀性能 |
| 陈园, 宫春波, 王胜刚, 马嵩, 张志东 |
|
Microstructure, Microhardness, and Corrosion Resistance of Nanocrystalline 304 Stainless Steel Plates |
| CHEN Yuan, GONG Chunbo, WANG Shenggang, MA Song, ZHANG Zhidong |
| 图11 NSSP-304样品的EBSD表征 |
| Fig.11 EBSD characterization of NSSP-304 sample (The color bands in pole figures and inverse pole figures denote the variation of pole density, the same in Fig.12) (a) crystal orientation map (b) misorientation angle distribution (c) {100}, {110}, and {111} pole figures (d) {100}, {110}, and {111} inverse pole figures |
|