纳米晶304不锈钢板材的微观组织、显微硬度与耐腐蚀性能
陈园, 宫春波, 王胜刚, 马嵩, 张志东

Microstructure, Microhardness, and Corrosion Resistance of Nanocrystalline 304 Stainless Steel Plates
CHEN Yuan, GONG Chunbo, WANG Shenggang, MA Song, ZHANG Zhidong
图6 NSSP-304和CPSS-304样品RD-TD、TD-ND和RD-ND面上的显微硬度平均值(不同线相同位置平均值)
Fig.6 Average microhardnesses (the same position N on different lines) of NSSP-304 and CPSS-304 samples on the RD-TD plane, TD-ND plane, and RD-ND plane