纳米晶304不锈钢板材的微观组织、显微硬度与耐腐蚀性能 |
| 陈园, 宫春波, 王胜刚, 马嵩, 张志东 |
|
Microstructure, Microhardness, and Corrosion Resistance of Nanocrystalline 304 Stainless Steel Plates |
| CHEN Yuan, GONG Chunbo, WANG Shenggang, MA Song, ZHANG Zhidong |
| 图4 NSSP-304和CPSS-304样品在0.5 mol/L HCl (室温)和6%FeCl3溶液(35 ℃)中的均匀腐蚀和点腐蚀性能 |
| Fig.4 Uniform and pitting corrosion properties of NSSP-304 and CPSS-304 samples in 0.5 mol/L HCl (at room temperature) (a-c) and 6%FeCl3 solutions (at 35 oC) (d-f) (i and t denote current density and time, respectively; k1-k5 are the slopes of curves in Fig.4d within different time ranges) (a) potentiostatic polarization curves in 0.5 mol/L HCl solution and partially enlarged view (inset) (b, c) surface SEM images of corroded NSSP-304 (b) and CPSS-304 (c) samples after the potentiostatic polarization (d) mass loss curves of NSSP-304 and CPSS-304 samples during immersion test in 6%FeCl3 solution (e, f) surface SEM images of corroded NSSP-304 (e) and CPSS-304 (f) samples after the immersion test |
|