Mo含量对1000 MPa级高强钢焊缝金属组织和力学性能的影响
刘洋, 孙健, 陆善平

Effect of Mo Content on the Microstructure and Mechanical Properties of 1000 MPa Grade High-Strength Steel Weld Metal
LIU Yang, SUN Jian, LU Shanping
图10 不同Mo含量焊缝金属的力学性能
Fig.10 Mechanical properties of weld metals with different Mo contents
(a) tensile properties at room temperature (Rp0.2—yield strength, Rm—tensile strength, A—elongation, Z—reduction of area)
(b) Vickers hardnesses (c) impact energies at room temperature