刘洋, 孙健, 陆善平

Effect of Mo Content on the Microstructure and Mechanical Properties of 1000 MPa Grade High-Strength Steel Weld Metal
LIU Yang, SUN Jian, LU Shanping
图7 不同Mo含量焊缝金属的XRD谱