贝氏体钢轨的低温疲劳裂纹扩展行为
刘蓉, 高古辉, 桂晓露, 白秉哲

Low-Temperature Fatigue Crack Propagation Behavior of Bainitic Rail Steel
LIU Rong, GAO Guhui, GUI Xiaolu, BAI Bingzhe
表2 贝氏体钢轨在不同温度下疲劳裂纹扩展速率的Paris方程
Table 2 Paris equations for da / dN of bainitic rail steel at different temperatures
TParis equationR2
RTda / dN = 4.87 × 10-9ΔK3.3870.998
-40 oCda / dN = 5.80 × 10-10ΔK4.0330.996