瞬态热处理对船用钛/钢接头界面组织和结合性能的影响 |
| 苏逸云, 郝晓虎, 黎书华, 崔泽琴, 闫德俊, 李卫国 |
|
Effect of Transient Heat Treatment on the Interfacial Microstructure and Bonding Properties of Titanium/Steel Transit Joint |
| SU Yiyun, HAO Xiaohu, LI Shuhua, CUI Zeqin, YAN Dejun, LI Weiguo |
| 图10 不同温度STHT前后钛/钢接头断口形貌及断裂处的SEM像和EDS面扫描图 |
| Fig.10 SEM images showing the fracture morphologies (a-c) and fracture positions (d-f) of titanium/steel transit joint as-welded (a, d) and after STHT under 600 oC (b, e) and 700 oC (c, f) (Insets in Figs.10a1-a3 and Figs.10d-f show the locally enlarged images of square regions and EDS mappings, respectively) |
|