瞬态热处理对船用钛/钢接头界面组织和结合性能的影响
苏逸云, 郝晓虎, 黎书华, 崔泽琴, 闫德俊, 李卫国

Effect of Transient Heat Treatment on the Interfacial Microstructure and Bonding Properties of Titanium/Steel Transit Joint
SU Yiyun, HAO Xiaohu, LI Shuhua, CUI Zeqin, YAN Dejun, LI Weiguo
图9 不同温度STHT前后钛/钢接头界面的黏结强度和剪切强度
Fig.9 Bonding strengths (a) and shear strengths (b) of the interface in titanium/steel transit joint as-welded and after STHT under different temperatures