瞬态热处理对船用钛/钢接头界面组织和结合性能的影响 |
| 苏逸云, 郝晓虎, 黎书华, 崔泽琴, 闫德俊, 李卫国 |
|
Effect of Transient Heat Treatment on the Interfacial Microstructure and Bonding Properties of Titanium/Steel Transit Joint |
| SU Yiyun, HAO Xiaohu, LI Shuhua, CUI Zeqin, YAN Dejun, LI Weiguo |
| 图7 不同温度STHT前后钛/钢接头界面局部取向差(KAM)图和平均取向差分布 |
| Fig.7 Kernel average misorientation (KAM) maps (a, c, e) and average misorientation distributions (b, d, f) of the interface in titanium/steel transit joint as-welded (a, b) and after STHT under 600 oC (c, d) and 700 oC (e, f) |
|