瞬态热处理对船用钛/钢接头界面组织和结合性能的影响 |
| 苏逸云, 郝晓虎, 黎书华, 崔泽琴, 闫德俊, 李卫国 |
|
Effect of Transient Heat Treatment on the Interfacial Microstructure and Bonding Properties of Titanium/Steel Transit Joint |
| SU Yiyun, HAO Xiaohu, LI Shuhua, CUI Zeqin, YAN Dejun, LI Weiguo |
| 图6 不同温度STHT前后钛/钢接头界面的晶界分布及晶界取向差统计图 |
| Fig.6 EBSD images (a, c, e) and grain boundary misorientation distributions (b, d, f) of the interface in titanium/steel transit joint as-welded (a, b) and after STHT under 600 oC (c, d) and 700 oC (e, f) (The black and red lines denote the high angle grain boundaries (HAGBs) with misorientation angle > 15° and low angle grain boundaries (LAGBs) with misorientation angle 2°-15°, respectively) |
|