瞬态热处理对船用钛/钢接头界面组织和结合性能的影响
苏逸云, 郝晓虎, 黎书华, 崔泽琴, 闫德俊, 李卫国

Effect of Transient Heat Treatment on the Interfacial Microstructure and Bonding Properties of Titanium/Steel Transit Joint
SU Yiyun, HAO Xiaohu, LI Shuhua, CUI Zeqin, YAN Dejun, LI Weiguo
图2 不同温度模拟瞬态热处理(STHT)前后钛/钢接头界面微观组织的SEM像
Fig.2 SEM images showing the interfacial microstructures (a1-d1), enlarged images of the straight interface (a2-d2), and enlarged images of non-straight interface (a3-d3) in titanium/steel transit joint as-welded (a1-a3) and after STHT under 400 oC (b1-b3), 600 oC (c1-c3), and 700 oC (d1-d3)