瞬态热处理对船用钛/钢接头界面组织和结合性能的影响 |
| 苏逸云, 郝晓虎, 黎书华, 崔泽琴, 闫德俊, 李卫国 |
|
Effect of Transient Heat Treatment on the Interfacial Microstructure and Bonding Properties of Titanium/Steel Transit Joint |
| SU Yiyun, HAO Xiaohu, LI Shuhua, CUI Zeqin, YAN Dejun, LI Weiguo |
| 图1 实验过程示意图 |
| Fig.1 Illustrations of the experiment process (a) explosive welding (Vd—detonation velocity, Vc—impact velocity, Vp—plate collision velocity, β—impact angle) (b) simulated transient heat treatment (STHT) experiment (c1, c2) shear strength (c1) and bonding strength (c2) tests (F—applied force) |
|