TC4钛合金激光表面重熔层内拉伸变形$\{10\bar{1}2\}$孪晶形成机制及马氏体变体选择规律
杨朋飞, 孙磊, 孙奇, 杨志远, 赵元, 高英, 张嘉振

Formation Mechanism of $\{10\bar{1}2\}$ Twins and Selection Rule of Martensitic Variants During Tensile Deformation in TC4 Titanium Alloy Laser Surface Remelting Layer
YANG Pengfei, SUN Lei, SUN Qi, YANG Zhiyuan, ZHAO Yuan, GAO Ying, ZHANG Jiazhen
表3 TC4钛合金中通过Burgers取向关系由β→α相变产生的12种变体[9,23,24]
Table 3 Twelve α variants in TC4 titanium alloy resulting from the β→α phase transition calculated by Burgers orientation relationship[9,23,24]
VariantPlane parallelDirection parallelRotation angle/axis from V1
V111¯0β//0001α111β//112¯0α-
V211¯0β//0001α111¯β//112¯0α10.53°/0001
V3110β//0001α11¯1β//112¯0α90°/1 2.38¯ 1.38 0
V4110β//0001α1¯11β//112¯0α90°/1 2.38¯ 1.38 0
V5101¯β//0001α11¯1β//112¯0α60.83°/1.377¯ 1 2.377 0.359
V6101¯β//0001α111β//112¯0α60°/112¯0
V7011¯β//0001α1¯11β//112¯0α60.83°/1.377¯ 1 2.377 0.359
V8011¯β//0001α111β//112¯0α60°/112¯0
V9011β//0001α11¯1β//112¯0α63.26°/10¯ 5 5 3¯
V10011β//0001α111¯β//112¯0α60.83°/1.377¯ 1 2.377 0.359
V11101β//0001α1¯11β//112¯0α63.26°/10¯ 5 5 3¯