均质化温度对3003铝合金微观组织和力学性能的影响规律
刘泽田, 路伟昭, 徐新宇, 刘旭, 张少游, 王慧远

Effect of Homogenization Temperature on the Microstructure and Mechanical Properties of 3003 Aluminum Alloys
LIU Zetian, LU Weizhao, XU Xinyu, LIU Xu, ZHANG Shaoyou, WANG Huiyuan
图8 3003铝合金的凝固路径(Scheil模型),计算得到的溶质分配系数和fcc相中溶质元素质量分数随固相分数的变化情况,铸态试样微观组织形貌,及实际凝固组织晶内溶质元素的质量分数分布规律
Fig.8 Solidification path of 3003 alloys in Scheil approximation (L—liquid) (a); evolution of solute partition coefficients (ki, i = Mn, Cu, Si, and Fe, the same below) (b) and solute concentrations (wi ) in fcc phases (c) with solid fraction calculated by Pandat software; the casting microstructure (d) and EDS results of Mn (e), Cu (f), Si (g), and Fe (h) along the line in Fig.8d