均质化温度对3003铝合金微观组织和力学性能的影响规律
刘泽田, 路伟昭, 徐新宇, 刘旭, 张少游, 王慧远

Effect of Homogenization Temperature on the Microstructure and Mechanical Properties of 3003 Aluminum Alloys
LIU Zetian, LU Weizhao, XU Xinyu, LIU Xu, ZHANG Shaoyou, WANG Huiyuan
图3 不同状态下3003铝合金的TEM像及EDS结果
Fig.3 TEM images (a, b) and corresponding EDS results (c, d) of 3003 aluminum alloy (a, c) LT sample (b, d) HT sample