TA18合金铸锭-管坯组织遗传行为及力学性能调控
李帅雨, 刘泽栋, 杨劼人, 金伟, 彭博, 杜新, 周斯曼

Microstructural Inheritance Behavior and Mechanical Property Control of TA18 Alloy From Ingot to Tube Blank
LI Shuaiyu, LIU Zedong, YANG Jieren, JIN Wei, PENG Bo, DU Xin, ZHOU Siman
图8 TA18合金热加工过程中的EBSD分析和晶体取向演变示意图
Fig.8 EBSD analyses (a-f, a1-a5) and schematics showing the evolution of crystal orientation (g) during thermomechanical processing (a-c) grain orientation spread (GOS) maps corresponding to the rough-forged (a), finish-forged (b), and extruded (c) conditions (a1, a2) enlarged GOS maps of the rectangle regions I (a1) and II (a2) in Fig.8a (G1-G5 represent different grains, and S1-S3 represent different subgrains) (a3) schematic of the crystal structures for subgrains S1-S3 marked in Fig.8a2 (a4, a5) misorientation angle profiles along lines L1 (a4) and L2 (a5) in Fig.8a2, respectively (d-f) PFs and IPFs corresponding to the rough-forged (d), finish-forged (e), and extruded (f) conditions