TA18合金铸锭-管坯组织遗传行为及力学性能调控 |
| 李帅雨, 刘泽栋, 杨劼人, 金伟, 彭博, 杜新, 周斯曼 |
|
Microstructural Inheritance Behavior and Mechanical Property Control of TA18 Alloy From Ingot to Tube Blank |
| LI Shuaiyu, LIU Zedong, YANG Jieren, JIN Wei, PENG Bo, DU Xin, ZHOU Siman |
| 图6 TA18合金铸锭不同部位与多阶段热加工后断口形貌的SEM像 |
| Fig.6 Low (a-f) and high (a1-f1) magnified SEM images of fracture morphologies of TA18 alloy ingot at different locations and after multi-stage hot processing (a, a1) edge of the ingot (b, b1) D / 4 position of the ingot (c, c1) D / 2 position of the ingot (d, d1) rough-forged bar (e, e1) finish-forged bar (f, f1) extruded billet |
|