TA18合金铸锭-管坯组织遗传行为及力学性能调控 |
| 李帅雨, 刘泽栋, 杨劼人, 金伟, 彭博, 杜新, 周斯曼 |
|
Microstructural Inheritance Behavior and Mechanical Property Control of TA18 Alloy From Ingot to Tube Blank |
| LI Shuaiyu, LIU Zedong, YANG Jieren, JIN Wei, PENG Bo, DU Xin, ZHOU Siman |
| 图5 TA18合金铸锭不同位置和多阶段热加工后的工程应力-应变曲线、力学性能对比和各强化机制对屈服强度的贡献 |
| Fig.5 Engineering stress-strain curves (a), mechanical properties (b), and contributions from several strengthening mechanisms to yield strength (c) of TA18 alloy ingots at different locations and after multi-stage hot processing (σρ —contribution of dislocation strengthening to yield strength, σH-P—contribution of fine grain strengthening to yield strength, σ0—matrix strength) |
|