TA18合金铸锭-管坯组织遗传行为及力学性能调控
李帅雨, 刘泽栋, 杨劼人, 金伟, 彭博, 杜新, 周斯曼

Microstructural Inheritance Behavior and Mechanical Property Control of TA18 Alloy From Ingot to Tube Blank
LI Shuaiyu, LIU Zedong, YANG Jieren, JIN Wei, PENG Bo, DU Xin, ZHOU Siman
图1 TA18合金加工流程示意图和拉伸样品尺寸
Fig.1 Schematic of thermomechanical processing route and dimension of tensile sample of TA18 alloy (unit: mm. AD—axial direction, CD—circumferential direction, RD—radial direction)