Nb4AlC3MAX 相单晶纳米线断面自修复原位定量研究 |
| 崔俊峰, 胡晓飞, 陈国新, 李友兵, 柯培玲, 赵宏伟 |
|
In Situ Quantification of Fracture Surface Self-Healing in Monocrystalline Nb4AlC3MAX Phase Nanowires |
| CUI Junfeng, HU Xiaofei, CHEN Guoxin, LI Youbing, KE Peiling, ZHAO Hongwei |
| 图5 修复前后Nb4AlC3MAX相纳米线断面的高分辨TEM像 |
| Fig.5 HRTEM images of fracture surfaces of the Nb4AlC3MAX phase nanowire before (a) and after (b) the self-healing, and after the irradiation-aided healing (c) (Arrows represent fracture surfaces) |
|