累积叠轧焊Cu/Nb多层材料中的滑移传递 |
| 杨然, 宋韶杰, 刘飞龙, 申熙美, 宋克兴, 刘峰 |
|
Slip Transfer in Accumulative Roll Bonding Cu/Nb Multilayer Composites |
| YANG Ran, SONG Shaojie, LIU Feilong, SHEN Ximei, SONG Kexing, LIU Feng |
| 图8 不同应变下Cu层与Nb层间相界(PB1)处的激活滑移系 (a) 0% (b) 4% (c) 8% (d) 12% |
| Fig.8 Activated slip systems at PB1 between Cu layer and Nb layer under different ε (PB—phase boundary) |
|