累积叠轧焊Cu/Nb多层材料中的滑移传递 |
| 杨然, 宋韶杰, 刘飞龙, 申熙美, 宋克兴, 刘峰 |
|
Slip Transfer in Accumulative Roll Bonding Cu/Nb Multilayer Composites |
| YANG Ran, SONG Shaojie, LIU Feilong, SHEN Ximei, SONG Kexing, LIU Feng |
| 图1 累积叠轧焊(ARB)工艺与原位拉伸试样尺寸示意图 |
| Fig.1 Schematics of accumulative roll bonding (ARB) procedure (a) and dimension of the in situ tensile sample (unit: mm) (b) |
|