表1 不同真应变时的材料常数
|
Table 1 Material constants at different true strains (ε)
|
|
| ε | Q / (J·mol-1) | lnA | n | α / MPa-1 |
|---|
| 0.10 | 155144.74 | 12.0671 | 2.8780 | 0.01426 | | 0.15 | 151640.37 | 11.8166 | 2.9379 | 0.01389 | | 0.20 | 145891.04 | 11.4170 | 2.9533 | 0.01375 | | 0.25 | 143261.63 | 11.0492 | 2.9686 | 0.01374 | | 0.30 | 140042.85 | 10.7365 | 2.9704 | 0.01373 | | 0.35 | 138616.43 | 10.6623 | 2.9957 | 0.01372 | | 0.40 | 135233.88 | 10.3218 | 2.9992 | 0.01371 | | 0.45 | 132736.45 | 10.0940 | 3.0369 | 0.01372 | | 0.50 | 129037.86 | 9.7158 | 3.0727 | 0.01375 | | 0.55 | 125617.22 | 9.3848 | 3.0967 | 0.01374 | | 0.60 | 121303.17 | 8.9610 | 3.1285 | 0.01372 | | 0.65 | 119952.93 | 8.8574 | 3.1801 | 0.01364 |
|
|
|