Ti551合金的热变形行为及热加工图构建 |
| 尹建年, 马英杰, 杨锐, 雷家峰, 齐敏, 周丽 |
|
Hot Deformation Behavior and Hot Processing Map Construction of the Ti551 Alloy |
| YIN Jiannian, MA Yingjie, YANG Rui, LEI Jiafeng, QI Min, ZHOU Li |
| 图4 Ti551合金在不同热压缩条件下的温度变化 |
| Fig.4 Temperature changes (ΔT) of Ti551 alloy at |
|