Zr-4合金带材冲制过程中的织构演变和变形机制:实验和宏微观耦合模拟研究 |
| 邓偲瀛, 董家瑄, 陈帅峰, 宋鸿武, 张士宏 |
|
Texture Evolution and Deformation Modes for Zr-4 Alloy During Stamping: Experiments and Modeling |
| DENG Siying, DONG Jiaxuan, CHEN Shuaifeng, SONG Hongwu, ZHANG Shihong |
| 图7 Zr-4冲制后样品纵截面实验与数值模拟厚度分布对比 |
| Fig.7 Comparisons of longitudinal cross-section thick-ness profile (a) and thickness distribution (b) of the Zr-4 stamped component between experi-mental and simulation results (Inset in Fig.7b shows the locations of the selected points) |
|