冲击加载下60钢的动态力学响应及层裂行为
杨坤, 郭庆伟, 李超, 张高龙, 赵宇宏, 侯华

Dynamic Mechanical Response and Spallation Behavior of 60 Steel Under Shock Loading
YANG Kun, GUO Qingwei, LI Chao, ZHANG Gaolong, ZHAO Yuhong, HOU Hua
表1 平板撞击实验参数
Table 1 Parameters of plate impact experiments
No.dfdsuf
mmmmkm·s-1
Shot 11.4922.9950.205
Shot 21.5023.0080.307
Shot 31.4932.9920.534
Shot 41.5093.0070.645