冲击加载下60钢的动态力学响应及层裂行为 |
| 杨坤, 郭庆伟, 李超, 张高龙, 赵宇宏, 侯华 |
|
Dynamic Mechanical Response and Spallation Behavior of 60 Steel Under Shock Loading |
| YANG Kun, GUO Qingwei, LI Chao, ZHANG Gaolong, ZHAO Yuhong, HOU Hua |
| 图11 Shot 3回收样品的SEM及EBSD表征结果 (a) SEM image (b) band contrast map (Arrows indicate microvoids located on twin boundaries) (c) IPF map (d) {112} and {111} PFs of the matrix and twins indicated by the black circle in Fig.11c |
| Fig.11 SEM and EBSD characterizations of the postmortem sample for Shot 3 |
|