冲击加载下60钢的动态力学响应及层裂行为
杨坤, 郭庆伟, 李超, 张高龙, 赵宇宏, 侯华

Dynamic Mechanical Response and Spallation Behavior of 60 Steel Under Shock Loading
YANG Kun, GUO Qingwei, LI Chao, ZHANG Gaolong, ZHAO Yuhong, HOU Hua
图10 C6~C8裂纹(图9)的SEM像和反极图的放大图