冲击加载下60钢的动态力学响应及层裂行为 |
| 杨坤, 郭庆伟, 李超, 张高龙, 赵宇宏, 侯华 |
|
Dynamic Mechanical Response and Spallation Behavior of 60 Steel Under Shock Loading |
| YANG Kun, GUO Qingwei, LI Chao, ZHANG Gaolong, ZHAO Yuhong, HOU Hua |
| 图8 微裂纹扩展方向与渗碳体片层方向之间的夹角角度分布 |
| Fig.8 Distributions of the angle between microcrack propagation direction and cementite lamellae direction |
|