基于固溶元素增材制造镍基高温合金的成分设计
张雪, 梁静静, 赵玉淞, 章环, 穆亚航, 周亦胄, 孙晓峰, 李金国

Design of Additively Manufactured Ni-Based Superalloys Based on Solid Solution Elements
ZHANG Xue, LIANG Jingjing, ZHAO Yusong, ZHANG Huan, MU Yahang, ZHOU Yizhou, SUN Xiaofeng, LI Jinguo
图5 合金固溶强度与裂纹面积分数的关系
Fig.5 Relationships between solid solution strength (σsss) and area fraction of cracks of alloys