超声功率对W90/Sn/Mg接头微观组织和力学性能的影响
张旭东, 付伟, 宋晓国, 宋娜, 孙浩, 胡胜鹏

Effect of Ultrasonic Power on the Microstructure and Mechanical Property of W90/Sn/Mg Joint
ZHANG Xudong, FU Wei, SONG Xiaoguo, SONG Na, SUN Hao, HU Shengpeng
表1 图2中标记点的化学成分及相种类 (atomic fraction / %)
Table 1 Chemical compositions and possible phases of spots marked in Fig.2a
PositionSnMgWNiFePhase type
A'0.010.0310.5464.2325.19(Ni, Fe) phase
B'99.820.110.020.030.02β-Sn
C'30.9868.970.010.030.01Mg2Sn
D'29.3070.650.010.030.01Mg2Sn