超声功率对W90/Sn/Mg接头微观组织和力学性能的影响 |
| 张旭东, 付伟, 宋晓国, 宋娜, 孙浩, 胡胜鹏 |
|
Effect of Ultrasonic Power on the Microstructure and Mechanical Property of W90/Sn/Mg Joint |
| ZHANG Xudong, FU Wei, SONG Xiaoguo, SONG Na, SUN Hao, HU Shengpeng |
| 图10 接头形成机理图 (a) heating process (b) applying ultrasound (c) cavitation effect (d) elemental diffusion (e) turning off ultrasound (f) cooling process |
| Fig.10 Schematics of formation mechanism of joint |
|