激光诱导转移技术制备超精细导电图案研究进展
袁康, 曹文鑫, 孙春强, 王卓超, 王笑笑, 张宇民, 朱嘉琦

Research Progress on the Preparation of Ultrafine Conductive Patterns Using Laser-Induced Transfer Technology
YUAN Kang, CAO Wenxin, SUN Chunqiang, WANG Zhuochao, WANG Xiaoxiao, ZHANG Yumin, ZHU Jiaqi
图4 不同厚度磁控溅射银薄膜表面形貌的SEM像及对应的三维粗糙度分布图[65]
Fig.4 High (a-e) and low (f-j) magnified SEM images of surface morphologies of magnetron-sputtered Ag thin films with different thicknesses, and corresponding 3D roughness maps (k-o)[65] (Rz—surface roughness)