熔盐堆用镍基合金失效机理与改性策略研究进展
王优, 陈向阳, 王煦嘉, 汤春桃, 沈朝, 曾小勤

Progress in Failure Mechanisms and Modification Strategies of Nickel-Based Alloys for Molten Salt Reactors
WANG You, CHEN Xiangyang, WANG Xujia, TANG Chuntao, SHEN Zhao, ZENG Xiaoqin
图5 辐照耦合效应对材料老化的影响[36,38]
(a) microstructure change[36]
(b) GB change[38]
(c) induced segregation and carbide precipitation[38]
(d) accelerated dissolution corrosion[36]
Fig.5 Influence of irradiation coupling effect on material degradation