Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究
刘丹, 白静, 章羽, 郭珂良, 刘新, 左良

First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping
LIU Dan, BAI Jing, ZHANG Yu, GUO Keliang, LIU Xin, ZUO Liang
表3 Ni-(Co)-Mn-(Si)-Ti合金的弹性性能
Table 3 Elastic properties for Ni-(Co)-Mn-(Si)-Ti alloys
AlloyB / GPaY / GPaG / GPaPc / GPavB / G
Ni2Mn1.5Ti0.5148.7292.7933.2368.870.3964.48
Ni2Mn1.25Si0.25Ti0.5155.08113.3441.1259.630.3783.77
Ni1.75Co0.25Mn1.25Si0.25Ti0.5152.52109.5439.6854.910.3803.84