Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究
刘丹, 白静, 章羽, 郭珂良, 刘新, 左良

First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping
LIU Dan, BAI Jing, ZHANG Yu, GUO Keliang, LIU Xin, ZUO Liang
表2 Ni2 - x Co x Mn1.25Si0.25Ti0.5合金奥氏体和马氏体最近邻Mn-Mn和Co-Mn原子之间的距离 (nm)
Table 2 Nearest Mn-Mn and Co-Mn distances of austenite and martensite for Ni2 - x Co x Mn1.25Si0.25Ti0.5 alloys
Atom pairPhasex
0.1250.250.3750.50.625
Mn-MnAustenite0.2730.2690.2800.2810.291
Martensite0.2550.2560.2550.2560.256
Co-MnAustenite0.2530.2520.2520.2520.252
Martensite0.2500.2490.2480.2470.247