Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究
|
|
刘丹, 白静, 章羽, 郭珂良, 刘新, 左良
|
First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping
|
|
LIU Dan, BAI Jing, ZHANG Yu, GUO Keliang, LIU Xin, ZUO Liang
|
|
表1 Ni2 - x Co x Mn1.5 - y Si y Ti0.5 (0≤ x ≤ 0.625,y = 0.125和0.25)合金的平衡晶格常数
|
Table 1 Equilibrium lattice constants of Ni2 - x Co x Mn1.5 - y Si y Ti0.5 (0≤ x ≤ 0.625, y = 0.125 and 0.25) alloys
|
|
| Ni2 -x Co x Mn1.5 -y Si y Ti0.5 | | Austenite | | NM martensite |
|---|
| y | x | | a = b = c / nm | V / nm3 | | a / nm | b / nm | c / nm | V / nm3 | | 0 | 0 | | 0.5848[48] | 0.2000 | | 0.4498 | 0.4176 | 0.5124 | 0.1925 | | 0.125 | 0 | | 0.5839 | 0.1991 | | 0.4475 | 0.4172 | 0.5138 | 0.1919 | | 0.125 | | 0.5834 | 0.1985 | | 0.4461 | 0.4164 | 0.5143 | 0.1911 | | 0.25 | | 0.5826 | 0.1977 | | 0.4446 | 0.4159 | 0.5171 | 0.1912 | | 0.375 | | 0.5821 | 0.1973 | | 0.3770 | 0.3777 | 0.6784 | 0.1932 | | 0.5 | | 0.5811 | 0.1962 | | 0.3782 | 0.3794 | 0.6733 | 0.1932 | | 0.625 | | 0.5812 | 0.1963 | | 0.3805 | 0.3807 | 0.6661 | 0.1929 | | 0.25 | 0 | | 0.5828 | 0.1979 | | 0.4447 | 0.4182 | 0.5152 | 0.1916 | | 0.125 | | 0.5828 | 0.1979 | | 0.4439 | 0.4169 | 0.5154 | 0.1908 | | 0.25 | | 0.5807 | 0.1958 | | 0.4428 | 0.4163 | 0.5179 | 0.1909 | | 0.375 | | 0.5812 | 0.1963 | | 0.4406 | 0.4153 | 0.5185 | 0.1898 | | 0.5 | | 0.5806 | 0.1957 | | 0.4381 | 0.4151 | 0.5221 | 0.1899 | | 0.625 | | 0.5819 (FA) | 0.1970 (FA) | | 0.4375 | 0.4150 | 0.5227 | 0.1898 |
|
|
|