Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究 |
| 刘丹, 白静, 章羽, 郭珂良, 刘新, 左良 |
|
First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping |
| LIU Dan, BAI Jing, ZHANG Yu, GUO Keliang, LIU Xin, ZUO Liang |
| 图12 Ni2 - x Co x Mn1.25Si0.25Ti0.5 (0≤ x ≤ 0.625)合金奥氏体和马氏体的TDOS |
| Fig.12 TDOS of austenite and martensite for Ni2 - x Co x -Mn1.25Si0.25Ti0.5 (0≤ x ≤ 0.625) alloys |
|