Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究 |
| 刘丹, 白静, 章羽, 郭珂良, 刘新, 左良 |
|
First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping |
| LIU Dan, BAI Jing, ZHANG Yu, GUO Keliang, LIU Xin, ZUO Liang |
| 图10 Ni2Mn1.5 - y Si y Ti0.5(0≤ y ≤ 0.25)合金奥氏体和马氏体的总态密度(TDOS) |
| Fig.10 Total density of states (TDOS) of austenite and martensite for Ni2Mn1.5 - y Si y Ti0.5 (0≤ y ≤ 0.25) alloys (The light blue shaded regions indicate the distribution of electronic density of states near Fermi level (EF). Figs.10a2-c2 present zoom-in views of the shaded regions in Figs.10a1-c1, respectively) (a1, a2) y = 0 (b1, b2) y = 0.125 (c1, c2) y = 0.25 |
|