Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究
刘丹, 白静, 章羽, 郭珂良, 刘新, 左良

First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping
LIU Dan, BAI Jing, ZHANG Yu, GUO Keliang, LIU Xin, ZUO Liang
图9 Ni2 - x Co x Mn1.25Si0.25Ti0.5 (0≤ x ≤ 0.625)合金马氏体的原子磁矩
Fig.9 Atomic magnetic moments of martensite for Ni2 - x Co x Mn1.25Si0.25Ti0.5 (0≤ x ≤ 0.625) alloys
(a) Ni (b) Mn (c) Ti (d) Si (e) Co