Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究 |
| 刘丹, 白静, 章羽, 郭珂良, 刘新, 左良 |
|
First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping |
| LIU Dan, BAI Jing, ZHANG Yu, GUO Keliang, LIU Xin, ZUO Liang |
| 图8 Ni2 - x Co x Mn1.25Si0.25Ti0.5 (0≤ x ≤ 0.625)合金奥氏体的原子磁矩 |
| Fig.8 Atomic magnetic moments of austenite for Ni2 - x Co x Mn1.25Si0.25Ti0.5 (0≤ x ≤ 0.625) alloys (The numbers 0-5 represent the contens of Co for 0, 0.125, 0.25, 0.375, 0.5, and 0.625, respectively; the same in Fig.9) (a) Ni (b) Mn (c) Ti (d) Si (e) Co |
|