Co、Si共掺杂调控Ni-Mn-Ti合金马氏体相变、磁性能和力学性能的第一性原理研究 |
| 刘丹, 白静, 章羽, 郭珂良, 刘新, 左良 |
|
First-Principles Study on the Regulation of Martensitic Transformation and Magnetic and Mechanical Properties of Ni-Mn-Ti Alloy via Co and Si Codoping |
| LIU Dan, BAI Jing, ZHANG Yu, GUO Keliang, LIU Xin, ZUO Liang |
| 图5 Ni2 - x Co x Mn1.5 - y Si y Ti0.5(0≤ x ≤ 0.625)合金奥氏体和马氏体的形成能 |
| Fig.5 Formation energies of austenite and martensite in Ni2 - x Co x Mn1.5 - y Si y Ti0.5 (0≤ x ≤ 0.625) alloys (AFA—antiferromagnetic austenite, FM—ferro-magnetic martensite, AFM—antiferromagnetic martensite. Within the shaded region, ferromag-netic austenite has higher thermodynamic stability than antiferromagnetic austenite) (a) y = 0.125 (Inset shows the locally enlarged view of the elliptical region) (b) y = 0.25 |
|